name:ALCe10

time:2018-11-3 16:27:22


Introduction
name brand Alloy elements % use Add the amount Using temperature ℃ performance
Aluminum bronze

ALCu50

Cu48~52 Adjust alloy composition Needs vary 570~600 crispy
al-si ALSi20 Si18~20 Adjust alloy composition
Needs vary
700~800 crispy
Aluminum manganese ALMn10 Mn9~11 Adjust alloy composition
Needs vary
770~830 toughening
Aluminum manganese ALMn20 Mn18~22 Adjust alloy composition
Needs vary
780~850 toughening
Aluminum  titanium ALTi5 Ti4~6 Grain refinement to improve plasticity
Needs vary
1020~1070 Easy segregation
Aluminum  titanium ALTi10 Ti9~11 Grain refinement to improve plasticity Needs vary
1020~1070 Easy segregation
Aluminum and nickel ALTi10
Ni9~11 To improve the plastic Needs vary
680~730 toughening
Aluminium chromium ALCr5 Cr4~6 Improve plasticity and performance Needs vary
900~1000 Easy segregation
Aluminium chromium ALCr10 Cr9~11 Improve plasticity and performance
Needs vary
900~1000 Easy segregation
Aluminium chromium ALCr20 Cr18~22 Improve plasticity and performance
Needs vary
910~1020 Easy segregation
Aluminium zirconium ALZr5 Zr4~6 Improve plasticity and performance
Needs vary
800~850 Easy segregation
Aluminum  antimony ALSb4 Sb3~5 Improve plasticity and performance
Needs vary
660 Easy segregation
Aluminum  antimony ALSb10 Sb9~11 Improve plasticity and performance
Needs vary
660 Easy segregation
Aluminum and iron ALFe20 Fe18~22 Improve plasticity and performance
Needs vary
1020 crispy
Aluminum and beryllium ALBe1 Be0.9~1.2 Improve plasticity and performance
Needs vary
820 crispy
Aluminum and beryllium
ALBe3 Be2~4 Improve plasticity and performance
Needs vary
820 crispy
Aluminum and beryllium
ALBe5 Be4.5~5.5 Improve plasticity and performance
Needs vary
820 crispy
Aluminum boron ALB3 B2.5~3.5 Reduce the resistivity, improve the conductivity, grain refinement 2~4% 800 crispy
Aluminum titanium boron (piece/wire) ALTi5B1

Ti4.5~6   B0.9~1.2

Grain refinement 0.5~2‰ 800 Easy segregation
Rare earth aluminum ALRe10 Re9~11 Grain refinement
2~3‰
680 Easy segregation
Alti boron rare earth ALTi5B1Re10 Ti5B1Re10 Grain refinement
1~3‰
800 Easy segregation
Titanium aluminum carbon ALTi5C0.2 Ti5C0.2 Grain refinement
1~2‰
1020~1070 Easy segregation
Aluminum strontium ALSr10 Sr9~11 For long - term modification of aluminum - silicon alloys under 13% silicon 1~2‰
680~740 Easy segregation
Yttrium aluminum ALY5 Y4~6 Improve plasticity and performance 1~2‰
740~800 Easy segregation
Aluminum bismuth ALBi10 Bi9~11 Improve plasticity and increase fluidity 1~2‰
700~710 Easy segregation
Aluminum scandium ALSc2 Sc Adjust the alloy composition and improve the alloy performance Needs vary
700-800 toughening
Aluminum cobalt ALCo5 Co Adjust the alloy composition and improve the alloy performance Needs vary
720-750 toughening
Aluminum molybdenum ALMo5-10 Mo Adjust the alloy composition and improve the alloy performance Needs vary
720-750 toughening
Aluminum niobium ALNb10 Nb Increase fluidity and improve alloy performance Needs vary
690-750 toughening
Aluminum neodymium ALNd30 Nd Adjust the alloy composition and improve the alloy performance Needs vary
690-750 Easy segregation
Aluminum cerium ALCe10 Ce Adjust the alloy composition and improve the alloy performance Needs vary
690-750 Easy segregation
Aluminum cadmium ALCd5 / 10 Cd Adjust the alloy composition and improve the alloy performance Needs vary
690-750 toughening
Aluminum tellurium ALTe5 Te Adjust the alloy composition and improve the alloy performance Needs vary
710-740 crispy
The chemical composition and impurities of aluminum intermediate alloy ingots shall be manufactured according to the YS/ t282-2000 standard.