name:HT-Cr75 chromium additive

time:2018-11-3 15:00:17


Introduction
name brand Alloy elements % use Add the amount Melting temperature ℃ Add the amount
Aluminum bronze

ALCu50

Cu48~52 Adjust alloy composition Needs vary 570~600 crispy
al-si ALSi20 Si18~20 Adjust alloy composition
Needs vary
700~800 crispy
Aluminum manganese ALMn10 Mn9~11 Adjust alloy composition
Needs vary
770~830 toughening
Aluminum manganese
ALMn20 Mn18~22 Adjust alloy composition
Needs vary
780~850 toughening
Aluminum titanium ALTi5 Ti4~6 Grain refinement to improve plasticity
Needs vary
1020~1070 Easy segregation
Aluminum titanium ALTi10 Ti9~11 Grain refinement to improve plasticity Needs vary
1020~1070 Easy segregation
Aluminum and nickel ALTi10
Ni9~11 To improve the plastic Needs vary
680~730 toughening
Aluminium chromium ALCr5 Cr4~6 Improve plasticity and performance Needs vary
900~1000 Easy segregation
Aluminium chromium ALCr10 Cr9~11 Improve plasticity and performance
Needs vary
900~1000 Easy segregation
Aluminium chromium ALCr20 Cr18~22 Improve plasticity and performance
Needs vary
910~1020 Easy segregation
Aluminium zirconium ALZr5 Zr4~6 Improve plasticity and performance
Needs vary
800~850 Easy segregation
Aluminum antimony ALSb4 Sb3~5 Improve plasticity and performance
Needs vary
660 Easy segregation
Aluminum antimony ALSb10 Sb9~11 Improve plasticity and performance
Needs vary
660 Easy segregation
Aluminum and iron ALFe20 Fe18~22 Improve plasticity and performance
Needs vary
1020 crispy
Aluminum and beryllium ALBe1 Be0.9~1.2 Improve plasticity and performance
Needs vary
820 toughening
Aluminum and beryllium
ALBe3 Be2~4 Improve plasticity and performance
Needs vary
820 toughening
Aluminum and beryllium
ALBe5 Be4.5~5.5 Improve plasticity and performance
Needs vary
820 toughening
Aluminum boron ALB3 B2.5~3.5 Reduce the resistivity, improve the conductivity, grain refinement 2~4% 800 toughening
Aluminum titanium boron (piece/wire) ALTi5B1

Ti4.5~6   B0.9~1.2

Grain refinement 0.5~2‰ 800 Easy segregation
Rare earth aluminum ALRe10 Re9~11 Grain refinement
2~3‰
680 Easy segregation
Alti boron rare earth ALTi5B1Re10 Ti5B1Re10 Grain refinement
1~3‰
800 Easy segregation
Titanium aluminum carbon ALTi5C0.2 Ti5C0.2 Grain refinement
1~2‰
1020~1070 Easy segregation
Aluminum strontium ALSr10 Sr9~11 For long - term modification of aluminum - silicon alloys under 13% silicon 1~2‰
680~740 Easy segregation
Yttrium aluminum ALY5 Y4~6 Improve plasticity and performance 1~2‰
740~800 Easy segregation
Aluminum bismuth ALBi10 Bi9~11 Improve plasticity and increase fluidity 1~2‰
700~710 Easy segregation
The chemical composition and impurities of aluminum intermediate alloy ingots shall be manufactured according to the YS/ t282-2000 standard.